General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.2 g/cm³ Show Supplier Material materials with Densidad of 8.2 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.2 % Show Supplier Material materials with Aluminio of 0.2 % | max. | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. | |
Carbono | 0.025 % Show Supplier Material materials with Carbono of 0.025 % | max. | |
Cobalto | 1 % Show Supplier Material materials with Cobalto of 1 % | max. | |
Cobre | 1.5 - 3 % Show Supplier Material materials with Cobre of 1.5 - 3 % | ||
Cromo | 19.5 - 23.5 % Show Supplier Material materials with Cromo of 19.5 - 23.5 % | ||
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. | |
Hierro | balance | ||
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. | |
Molibdeno | 2.5 - 3.5 % Show Supplier Material materials with Molibdeno of 2.5 - 3.5 % | ||
Níquel | 38 - 46 % Show Supplier Material materials with Níquel of 38 - 46 % | ||
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. | |
Titanio | 0.6 - 1.2 % Show Supplier Material materials with Titanio of 0.6 - 1.2 % |