General
Property | Value | Comment |
---|---|---|
Recycled Content | 82.1 % Show Supplier Material materials with Recycled Content of 82.1 % | Average recycled content |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 35 % Show Supplier Material materials with Elongación of 35 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 270 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 270 MPa | min. |
Resistencia a la tracción | 23.0 °C | 550 - 750 MPa Show Supplier Material materials with Resistencia a la tracción of 550 - 750 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | max. | |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. | |
Cromo | 18.5 % Show Supplier Material materials with Cromo of 18.5 % | ||
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. | |
Hierro | Balance | ||
Manganeso | 1.3 % Show Supplier Material materials with Manganeso of 1.3 % | ||
Nitrógeno | 0.14 % Show Supplier Material materials with Nitrógeno of 0.14 % | ||
Níquel | 9 % Show Supplier Material materials with Níquel of 9 % | ||
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % |