General
Property | Value | Comment |
---|---|---|
Recycled Content | 82.1 % Show Supplier Material materials with Recycled Content of 82.1 % | Average recycled content |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 35 % Show Supplier Material materials with Elongación of 35 % | min. |
Límite elástico Rp 0,2 | 23.0 °C | 205 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 205 MPa | min. |
Resistencia a la tracción | 23.0 °C | 510 - 690 MPa Show Supplier Material materials with Resistencia a la tracción of 510 - 690 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. | |
Carbono | 0.06 % Show Supplier Material materials with Carbono of 0.06 % | max. | |
Cromo | 16.5 % Show Supplier Material materials with Cromo of 16.5 % | ||
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. | |
Hierro | Balance | ||
Manganeso | 1.3 % Show Supplier Material materials with Manganeso of 1.3 % | ||
Niobio | 0.7 % Show Supplier Material materials with Niobio of 0.7 % | ||
Níquel | 13 % Show Supplier Material materials with Níquel of 13 % | ||
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % |