Ceramic Silicon Carbide Composite SICAPRINT™ Si10

Want to keep this datasheet? Save it now in your required format

Description

Here we bring the excellent physical properties of silicon carbide into complex shapes.


The material base and the broad range of refinement processes allow us to produce tough industrial components with high heat resistance, high thermal conductivity and hardness. The different types of SICAPRINT Si give our customers the opportunity to choose the most economical type for their application.


The advantages of SICAPRINT™ Si are:

  • Temperature stability up to 1400 °C
  • Excellent thermal conductivity
  • High hardness

Los datos sobre este material han sido proporcionados por SGL Carbon.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueComment

Densidad

2.8 g/cm³

Show Supplier Material materials with Densidad of 2.8 g/cm³

Porosidad

0.1 %

Show Supplier Material materials with Porosidad of 0.1 %

open porosity, max

Mecánica

PropertyValue

Módulo elástico

270 GPa

Show Supplier Material materials with Módulo elástico of 270 GPa

Resistencia a la flexión

110 MPa

Show Supplier Material materials with Resistencia a la flexión of 110 MPa

Aplicaciones térmicas

PropertyValue

Conductividad térmica

120 W/(m·K)

Show Supplier Material materials with Conductividad térmica of 120 W/(m·K)

Eléctrico

PropertyValue

Resistividad eléctrica

7.5e-05 Ω·m

Show Supplier Material materials with Resistividad eléctrica of 7.5e-05 Ω·m

Technological properties

Property