SIGRATHERM® Water Based Graphite Dispersions Grade B
Description
Dispersions based on expanded graphite powders and graphite nanoplates.
Expanded graphite nanoplates consist of small, 1-15 nanometer thick, single or multilayer graphite layers, with diameters up to 100 micrometers. They constitute a new class of graphite nanoparticles with multifunctional properties. In order to obtain a graphite dispersion, small graphite particles and nanoplates produced by secondary treatment of our expanded graphite are mixed with a dispersant in water. Depending on the application, the viscosity of the dispersion can be adjusted by means of different concentrations of solids. The maximum dispersible solid content is 5.5% by weight.
Key characteristics of our graphite nanoplates are:
- Excellent layer formation on a variety of substrates, e.g. copper foil or PET film
- The high aspect ratio of the graphite nanoplates allows high electrical and thermal conductivity
- Freestanding graphite foils with a thickness between 5 and 15 μm can be produced
Los datos sobre este material han sido proporcionados por SGL Carbon.
A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.