General
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de permeabilidad | 20 °C | 0.25 cm²/s Show Supplier Material materials with Coeficiente de permeabilidad of 0.25 cm²/s | |
Densidad aparente | 1.77 g/cm³ Show Supplier Material materials with Densidad aparente of 1.77 g/cm³ | ||
Porosidad | 14.0 % Show Supplier Material materials with Porosidad of 14.0 % | open porosity | |
Tamaño de grano | 10.0 μm Show Supplier Material materials with Tamaño de grano of 10.0 μm |
Mecánica
Property | Value | Comment |
---|---|---|
Hardness, Rockwell | 70.0 [-] Show Supplier Material materials with Hardness, Rockwell of 70.0 [-] | 5/100 |
Módulo elástico | 10.5 GPa Show Supplier Material materials with Módulo elástico of 10.5 GPa | Dynamic Modulus |
Resistencia a la compresión | 110 MPa Show Supplier Material materials with Resistencia a la compresión of 110 MPa | |
Resistencia a la flexión | 50 MPa Show Supplier Material materials with Resistencia a la flexión of 50 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 4.2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.2e-06 1/K | @20-200°C | |
Conductividad térmica | 20 °C | 95 W/(m·K) Show Supplier Material materials with Conductividad térmica of 95 W/(m·K) | |
Contenido de cenizas | 0.02 % Show Supplier Material materials with Contenido de cenizas of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Metallurgical applications e.g. continuous casting, crucibles, sintering molds, etc. | |
Processing methods | Isostatically pressed |