General
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de permeabilidad | 20 °C | 0.15 cm²/s Show Supplier Material materials with Coeficiente de permeabilidad of 0.15 cm²/s | |
Densidad aparente | 1.82 g/cm³ Show Supplier Material materials with Densidad aparente of 1.82 g/cm³ | ||
Porosidad | 10.0 % Show Supplier Material materials with Porosidad of 10.0 % | open porosity | |
Tamaño de grano | 20.0 μm Show Supplier Material materials with Tamaño de grano of 20.0 μm |
Mecánica
Property | Value | Comment |
---|---|---|
Hardness, Rockwell | 100.0 [-] Show Supplier Material materials with Hardness, Rockwell of 100.0 [-] | 10/100 |
Módulo elástico | 11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | Dynamic Modulus |
Resistencia a la compresión | 105 MPa Show Supplier Material materials with Resistencia a la compresión of 105 MPa | |
Resistencia a la flexión | 50 MPa Show Supplier Material materials with Resistencia a la flexión of 50 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 4.2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.2e-06 1/K | @20-200°C | |
Conductividad térmica | 20 °C | 125 W/(m·K) Show Supplier Material materials with Conductividad térmica of 125 W/(m·K) | |
Contenido de cenizas | 0.01 % Show Supplier Material materials with Contenido de cenizas of 0.01 % |
Technological properties
Property | ||
---|---|---|
Application areas | Metallurgical applications e.g. continuous casting, crucibles, sintering molds, etc. | |
Processing methods | Isostatically pressed |