General
Property | Value | Comment |
---|---|---|
Coeficiente de permeabilidad | 0.01 cm²/s Show Supplier Material materials with Coeficiente de permeabilidad of 0.01 cm²/s | |
Densidad aparente | 1.88 g/cm³ Show Supplier Material materials with Densidad aparente of 1.88 g/cm³ | |
Porosidad | 10.0 % Show Supplier Material materials with Porosidad of 10.0 % | open porosity |
Tamaño de grano | 3.0 μm Show Supplier Material materials with Tamaño de grano of 3.0 μm |
Mecánica
Property | Value | Comment |
---|---|---|
Hardness, Rockwell | 105.0 [-] Show Supplier Material materials with Hardness, Rockwell of 105.0 [-] | 5/100 |
Módulo elástico | 13.5 GPa Show Supplier Material materials with Módulo elástico of 13.5 GPa | Dynamic Modulus |
Resistencia a la compresión | 170 MPa Show Supplier Material materials with Resistencia a la compresión of 170 MPa | |
Resistencia a la flexión | 85 MPa Show Supplier Material materials with Resistencia a la flexión of 85 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 4.7e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.7e-06 1/K | @20-200°C | |
Conductividad térmica | 20 °C | 100 W/(m·K) Show Supplier Material materials with Conductividad térmica of 100 W/(m·K) | |
Contenido de cenizas | 0.0005 % Show Supplier Material materials with Contenido de cenizas of 0.0005 % | depending on the code, it can also be less than 5 ppm | |
0.003 % Show Supplier Material materials with Contenido de cenizas of 0.003 % | depending on the code, it can also be less than 5 ppm |
Eléctrico
Property | Value |
---|---|
Resistividad eléctrica | 1.3000000000000001e-05 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.3000000000000001e-05 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 1e-06 - 5e-06 % Show Supplier Material materials with Aluminio of 1e-06 - 5e-06 % | depending on the code, it can also be less |
Boro | 2e-06 - 1e-05 % Show Supplier Material materials with Boro of 2e-06 - 1e-05 % | depending on the code, it can also be less |
Calcio | 1e-06 - 2e-05 % Show Supplier Material materials with Calcio of 1e-06 - 2e-05 % | depending on the code |
Cobalto | 1e-06 - 2e-06 % Show Supplier Material materials with Cobalto of 1e-06 - 2e-06 % | depending on the code, it can also be less |
Cobre | 1e-06 - 2e-06 % Show Supplier Material materials with Cobre of 1e-06 - 2e-06 % | depending on the code, it can also be less |
Cromo | 1e-06 - 2e-06 % Show Supplier Material materials with Cromo of 1e-06 - 2e-06 % | depending on the code, it can also be less |
Fósforo | 2e-06 - 1e-05 % Show Supplier Material materials with Fósforo of 2e-06 - 1e-05 % | depending on the code, it can also be less |
Hierro | 2e-06 - 5e-05 % Show Supplier Material materials with Hierro of 2e-06 - 5e-05 % | depending on the code |
Magnesio | 1e-06 - 1e-05 % Show Supplier Material materials with Magnesio of 1e-06 - 1e-05 % | depending on the code |
Manganeso | 1e-06 % Show Supplier Material materials with Manganeso of 1e-06 % | max. |
Níquel | 1e-06 - 0.0001 % Show Supplier Material materials with Níquel of 1e-06 - 0.0001 % | depending on the code, it can also be less |
Silicona | 0.0001 - 0.0002 % Show Supplier Material materials with Silicona of 0.0001 - 0.0002 % | depending on the code, it can also be less |
Titanio | 1e-06 - 2e-05 % Show Supplier Material materials with Titanio of 1e-06 - 2e-05 % | depending on the code |
Vanadio | 1e-06 - 5e-05 % Show Supplier Material materials with Vanadio of 1e-06 - 5e-05 % | depending on the code |
Technological properties
Property | ||
---|---|---|
Processing methods | Isostatically pressed |