General
Property | Value |
---|---|
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ |
Mecánica
Property | Value |
---|---|
Failure Strain | 1.2 % Show Supplier Material materials with Failure Strain of 1.2 % |
Módulo de flexión | 50 GPa Show Supplier Material materials with Módulo de flexión of 50 GPa |
Módulo elástico | 44 GPa Show Supplier Material materials with Módulo elástico of 44 GPa |
Resistencia a la flexión | 400 MPa Show Supplier Material materials with Resistencia a la flexión of 400 MPa |
Resistencia a la tracción | 570.0 MPa Show Supplier Material materials with Resistencia a la tracción of 570.0 MPa |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Components and assemblies based on plate material (liquid distributors, collectors, support grids, retainers) |