General
Property | Value |
---|---|
Densidad | 1.5 g/cm³ Show Supplier Material materials with Densidad of 1.5 g/cm³ |
Mecánica
Property | Value |
---|---|
Failure Strain | 0.4 % Show Supplier Material materials with Failure Strain of 0.4 % |
Módulo de flexión | 75 GPa Show Supplier Material materials with Módulo de flexión of 75 GPa |
Módulo elástico | 65 GPa Show Supplier Material materials with Módulo elástico of 65 GPa |
Resistencia a la flexión | 340 MPa Show Supplier Material materials with Resistencia a la flexión of 340 MPa |
Resistencia a la tracción | 270.0 MPa Show Supplier Material materials with Resistencia a la tracción of 270.0 MPa |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Components and assemblies based on plate material (liquid distributors, collectors, support grids, retainers) |