General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 1.25 % Show Supplier Material materials with Absorción de agua of 1.25 % | |
Densidad | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | ISO1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 6.5 % Show Supplier Material materials with Elongación of 6.5 % | ISO527 |
Módulo de flexión | 23.0 °C | 4.5 GPa Show Supplier Material materials with Módulo de flexión of 4.5 GPa | ISO178 |
Resistencia a la flexión | 23.0 °C | 175 MPa Show Supplier Material materials with Resistencia a la flexión of 175 MPa | ISO178 |
Resistencia a la tracción | 23.0 °C | 125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | ISO527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | ISO179 |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | ISO179 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ISO 75/A | |
Temperatura de fusión | 225 - 230 °C Show Supplier Material materials with Temperatura de fusión of 225 - 230 °C | ISO3146 | |
Inflamabilidad | HB UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | GB/T 1408 |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | GB/T1410 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, mechanical shields, blades, gears, power tools, etc. | |
Fillers | 18% Glass Fiber |