General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.12 g/cm³ | ISO1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | ISO527 |
Módulo de flexión | 23.0 °C | 6 GPa Show Supplier Material materials with Módulo de flexión of 6 GPa | ISO178 |
Resistencia a la flexión | 23.0 °C | 125 MPa Show Supplier Material materials with Resistencia a la flexión of 125 MPa | ISO178 |
Resistencia a la tracción | 23.0 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | ISO527 |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | ISO179 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, consumer goods, etc. | |
Fillers | 30% Glass Fiber |