General
Property | Value |
---|---|
Densidad | 2.61 g/cm³ Show Supplier Material materials with Densidad of 2.61 g/cm³ |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 9.2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9.2e-06 1/K | ISO 7991 | mean value for 20-300 °C |
Softening temperature | 675.0 °C Show Supplier Material materials with Softening temperature of 675.0 °C | ISO 7884-3 | Viscosity 10⁷·⁶ dPa·s |
Specific electrical resistance temperature | 280.0 °C Show Supplier Material materials with Specific electrical resistance temperature of 280.0 °C | For ρ=10⁸ Ω·cm | |
Temperatura de recocido | 480.0 °C Show Supplier Material materials with Temperatura de recocido of 480.0 °C | ISO 7884-4 | Viscosity 10¹³ dPa·s |
Temperatura de transición del vidrio | 470 °C Show Supplier Material materials with Temperatura de transición del vidrio of 470 °C | ISO 7884-8 | |
Working temperature | 1015.0 °C Show Supplier Material materials with Working temperature of 1015.0 °C | ISO 7884-2 | Viscosity 10⁴ dPa·s |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 250 °C | 3.98e+06 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.98e+06 Ω·m |
350 °C | 63096 Ω·m Show Supplier Material materials with Resistividad eléctrica of 63096 Ω·m |
Chemical properties
Property | ||
---|---|---|
Other | 0.01 % | max., Lead, Cadmium, Mercury and Hexavalent Chromium |
Technological properties
Property | ||
---|---|---|
Application areas | Glass suitable for bodies of glass electrodes (tubes for pH electrodes), Sealing glass for special lightning. | |
Corrosion properties | Hydrolytic resistance Class HGB3 (ISO 719) - Acid resistance Class S1 (DIN 12116) - Alkali resistance Class A2 (ISO695) |