General
Property | Value |
---|---|
Densidad | 2.77 g/cm³ Show Supplier Material materials with Densidad of 2.77 g/cm³ |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 6.6e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.6e-06 1/K | ISO 7991 | mean value for 20-300 °C |
Temperatura de transición del vidrio | 635 °C Show Supplier Material materials with Temperatura de transición del vidrio of 635 °C | ISO 7884-8 | |
Working temperature | 1100.0 °C Show Supplier Material materials with Working temperature of 1100.0 °C | ISO 7884-2 | Viscosity 10⁴ dPa·s |
Chemical properties
Property | ||
---|---|---|
Other | 0.01 % | max., Lead, Cadmium, Mercury and Hexavalent Chromium |
Technological properties
Property | ||
---|---|---|
Application areas | Signal intensifier, detector and (fibre-) optics and other electrotechnology/electronics. | |
Corrosion properties | Hydrolytic resistance Class HGB2 (ISO 719) - Acid resistance Class S2 (DIN 12116) - Alkali resistance Class A1 (ISO695) |