General
Property | Value |
---|---|
Densidad | 2.25 g/cm³ Show Supplier Material materials with Densidad of 2.25 g/cm³ |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 3.8e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.8e-06 1/K | ISO 7991 | mean value for 20-300 °C |
Softening temperature | 800.0 °C Show Supplier Material materials with Softening temperature of 800.0 °C | ISO 7884-3 | Viscosity 10⁷·⁶ dPa·s |
Specific electrical resistance temperature | 265.0 °C Show Supplier Material materials with Specific electrical resistance temperature of 265.0 °C | For ρ=10⁸ Ω·cm | |
Temperatura de recocido | 560.0 °C Show Supplier Material materials with Temperatura de recocido of 560.0 °C | ISO 7884-4 | Viscosity 10¹³ dPa·s |
Temperatura de transición del vidrio | 510 °C Show Supplier Material materials with Temperatura de transición del vidrio of 510 °C | ISO 7884-8 | |
Working temperature | 1210.0 °C Show Supplier Material materials with Working temperature of 1210.0 °C | ISO 7884-2 | Viscosity 10⁴ dPa·s |
Óptico
Property | Value | Comment |
---|---|---|
Índice de refracción | 1.5 [-] Show Supplier Material materials with Índice de refracción of 1.5 [-] | at λ=587.6 nm |
Technological properties
Property | ||
---|---|---|
Application areas | Transmitter and x-ray tubes, other Electrotechnology/Electronics | |
Corrosion properties | Hydrolytic resistance Class HGB1 (ISO 719) |