General
Property | Value |
---|---|
Densidad | 3.18 g/cm³ Show Supplier Material materials with Densidad of 3.18 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 4.5e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.5e-06 1/K | ISO 7991 | mean value for 20-300 °C | |
Conductividad térmica | 90 °C | 0.9 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.9 W/(m·K) | ||
Softening temperature | 638.0 °C Show Supplier Material materials with Softening temperature of 638.0 °C | ISO 7884-3 | Viscosity 10⁷·⁶ dPa·s | |
Temperatura de recocido | 490.0 °C Show Supplier Material materials with Temperatura de recocido of 490.0 °C | ISO 7884-4 | Viscosity 10¹³ dPa·s | |
Temperatura de transición del vidrio | 495 °C Show Supplier Material materials with Temperatura de transición del vidrio of 495 °C | ISO 7884-8 | ||
Working temperature | 900.0 °C Show Supplier Material materials with Working temperature of 900.0 °C | ISO 7884-2 | Viscosity 10⁴ dPa·s |
Eléctrico
Property | Value | Frequency |
---|---|---|
Constante dieléctrica | 6.9 [-] Show Supplier Material materials with Constante dieléctrica of 6.9 [-] | 1MHz |
Tangente de pérdidas | 0.0035 [-] Show Supplier Material materials with Tangente de pérdidas of 0.0035 [-] | 1MHz |
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Stress optical coefficient | 3.4e-06 mm²/N Show Supplier Material materials with Stress optical coefficient of 3.4e-06 mm²/N | DIN 52314 | |
Índice de refracción | 1.6 [-] Show Supplier Material materials with Índice de refracción of 1.6 [-] | at λ=587.6 nm |
Technological properties
Property | ||
---|---|---|
Application areas | For power and pin diodes as well as microdiodes, Signal intensifier, detector (other Electrotechnology/Electronics), Sensors | |
Corrosion properties | Hydrolytic resistance Class HGB1 (ISO 719) - Acid resistance Class S4 (DIN 12116) - Alkali resistance Class A3 (ISO695) |