General
Property | Temperature | Value | Comment |
---|---|---|---|
Bio-based content | 30.0 % Show Supplier Material materials with Bio-based content of 30.0 % | ||
Densidad | 23 °C | 1.02 g/cm³ Show Supplier Material materials with Densidad of 1.02 g/cm³ | ISO 1183 |
Recycled Content | 70.0 % Show Supplier Material materials with Recycled Content of 70.0 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23 °C | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | ISO 527-2/50 |
Módulo de flexión | 23 °C | 2.8 GPa Show Supplier Material materials with Módulo de flexión of 2.8 GPa | ISO 527-2/2 |
Módulo elástico | 23 °C | 3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | ISO 527-2/2 |
Resistencia a la tracción | 23 °C | 36 MPa Show Supplier Material materials with Resistencia a la tracción of 36 MPa | ISO 527-2/50 |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 16 kJ/m² | ISO 179/1eU |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL94: HB |
Technological properties
Property | ||
---|---|---|
Certifications | ||
Fillers | 30% S-Wood Fiber | |
Other | General safety instructions, read also Process instructions: | |
Processing methods | Drying: 4 hours at 105°C Injection moulding machine Temperatures: The below instructions may differ on due to injection speed, machine etc. Read process intructions. |