General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.09 g/cm³ Show Supplier Material materials with Densidad of 1.09 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 9 % Show Supplier Material materials with Elongación of 9 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 10.2 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 10.2 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 1.5 GPa Show Supplier Material materials with Módulo de flexión of 1.5 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 47 MPa Show Supplier Material materials with Resistencia a la flexión of 47 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 28 MPa Show Supplier Material materials with Resistencia a la tracción of 28 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 83 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 83 °C | ASTM D648 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+7 - 1.00E+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+7 - 1.00E+10 Ω/sq | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.9 % Show Supplier Material materials with Contracción of 0.9 % | ASTM D1238, Mold Shrinkage |
Velocidad de flujo de la masa derretida | 3.72 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3.72 g/10min | ASTM D1238, 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hard drive and memory fixtures, Computer work surfaces, ESD circular disc, ESD protection board, ESD electric & housing spare parts, Electric accessories | |
Certifications | RoHS | |
Color | Black | |
Processing methods | Injection molding - Drying time: 4hrs, temperature: 85°C - injection temperature: 200-230°C |