Tribotecc® Fibratecc® SF 150 Functional Fibers, Steel fibers
Description
Tribotecc® Fibratecc® SF 150 is a solid lubricant based on functional steel fibers and iron sulfide. The key benefits of Tribotecc® Fibratecc® SF 150 are:
A significant decrease of friction resistance
by functional fibers that are coated with metal sulfides
Therefore less powder solid lubricant is needed
Excellent tribological characteristics: The fibers form contact plateaus at those points where friction occurs. Because the fibers are coated with a lubricating layer of metal sulfides, they are wear-resistant
A strong reduction of dust, especially respirable particles
The non-use of Cu- and Sb
Forms protective layers of different contact surfaces over a wide temperature and pressure range
Fiber Information | Length (mm) | Diameter (mm) |
---|
Average | 1.9 | 0.05 |
Minimum | 1 | 0.02 |
Maximum | 3.3 | 0.1 |
Los datos sobre este material han sido proporcionados por Tribotecc.
A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.