General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.07 % Show Supplier Material materials with Absorción de agua of 0.07 % | @24 hours | ASTM D570 |
Densidad | 23.0 °C | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % | ASTM D638 |
Flexural yield strength | 23.0 °C | 14 MPa Show Supplier Material materials with Flexural yield strength of 14 MPa | ASTM D790 |
Hardness, Rockwell R | 23.0 °C | 119 [-] Show Supplier Material materials with Hardness, Rockwell R of 119 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | -40.0 °C | 133 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 133 J/m | ASTM D256 |
20.0 °C | 187 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 187 J/m | ASTM D256 | |
Módulo de flexión | 23.0 °C | 2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 63.4 MPa Show Supplier Material materials with Resistencia a la tracción of 63.4 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6E-5 1/K | ASTM E831 | ||
Heat deflection temperature, 0.45 MPa | 123 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 123 °C | ASTM D648 | |||
Inflamabilidad | UL94: V-1 for 1.5mm and V-0 for V-0 for 6mm |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.69 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.69 [-] | ASTM D150 |
Dissipation factor, 60Hz | 23.0 °C | 7E-4 [-] Show Supplier Material materials with Dissipation factor, 60Hz of 7E-4 [-] | ASTM D150 |
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | ASTM D149 |