General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20.0 °C | 4.56 g/cm³ Show Material materials with Densidad of 4.56 g/cm³ | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elongación | 20.0 °C | 25.0 % Show Material materials with Elongación of 25.0 % | Solution Annealed | WL 3.7124-1 | Forging, Rod |
Estricción | 20.0 °C | 45.0 Show Material materials with Estricción of 45.0 | Solution Annealed | WL 3.7124-1 | Forging, Rod |
Módulo elástico | 20.0 °C | 113.0 GPa Show Material materials with Módulo elástico of 113.0 GPa | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |
Resistencia a la tracción | 20.0 °C | 620.0 MPa Show Material materials with Resistencia a la tracción of 620.0 MPa | Solution Annealed | WL 3.7124-1 | Flat |
20.0 °C | 640.0 MPa Show Material materials with Resistencia a la tracción of 640.0 MPa | Solution Annealed | WL 3.7124-1 | Forging, Rod |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 460.0 - 527.0 J/(kg·K) Show Material materials with Calor específico of 460.0 - 527.0 J/(kg·K) | Typical for Titanium Alpha Alloy |
Coeficiente de dilatación térmica | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Alpha Alloy |
Conductividad térmica | 4.0 - 17.0 W/(m·K) Show Material materials with Conductividad térmica of 4.0 - 17.0 W/(m·K) | Typical for Titanium Alpha Alloy |
Temperatura de fusión | 1540.0 - 1715.0 °C Show Material materials with Temperatura de fusión of 1540.0 - 1715.0 °C | Typical for Titanium Alpha Alloy |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbono | 0.1 Show Material materials with Carbono of 0.1 | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |
Cobre | 2.0 - 3.0 % Show Material materials with Cobre of 2.0 - 3.0 % | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |
Hidrógeno | 0.01 Show Material materials with Hidrógeno of 0.01 | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |
Hierro | 0.2 Show Material materials with Hierro of 0.2 | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |
Oxígeno | 0.2 Show Material materials with Oxígeno of 0.2 | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |
Titanio | 96.4 % Show Material materials with Titanio of 96.4 % | Solution Annealed | WL 3.7124-1 | Forging, Rod, Flat |