Acerinox is one of the most competitive companies in the world in the manufacturing of stainless steels and nickel alloys.
Sede
Madrid, Spain
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
, ISO 50001
, ISO 14001
Grade | Shape | ||
---|---|---|---|
EN 1.4016 | Billet | EN 1.4016, EN X6Cr17, AISI 430 | EN 10088 |
EN 1.4031 | Disc | EN 1.4031, EN X39Cr13, AISI 420 | EN 10088 |
EN 1.4104 | Bar | EN 1.4104, EN X14CrMoS17 | |
EN 1.4105 | Billet | EN 1.4105, EN X6CrMoS17, AISI 430F | EN 10088 |
EN 1.4113 | Billet | EN 1.4113, EN X6CrMo17-1, AISI 434 | EN 10088 |
EN 1.4116 | Disc | EN 1.4116, EN X50CrMoV15, AISI 420MoV | EN 10088 |
EN 1.4301 | Billet | EN 1.4301, EN X5CrNi18-10, AISI 304 | EN 10088 |
EN 1.4303 | Billet | EN 1.4303, EN X4CrNi18-12, AISI 305 | EN 10088 |
EN 1.4305 | Billet | EN 1.4305, EN X8CrNiS18-9, AISI 303 | EN 10088 |
EN 1.4306 | Billet | EN 1.4306, EN X2CrNi19-11, AISI 304L | EN 10088 |