S+D customers should be able to make the best decisions possible during the material selection stage of the design process. That is why our customers are served by experienced product specialists with extensive industry experience. We are a global company with an international team that is united by the shared values of our corporate philosophy. We are not only concerned about selling our competitive products, but also about long-lasting and trusting business relationships. True to our motto “Supporting Your Success”, we always focus on our customers and place great emphasis on the continuous optimization of our range of stock and services. This enables us to respond even more individually to customer requirements and create real added value for our customers through innovation, expertise, and just-in-time delivery.
Sede
Stelle, Germany
Sitio web
Tipo
Processor and Distributor
Certifications
ISO 9001
, EN 10204-3.1
, DIN EN 9120
, ISO 14001
Grade | Shape | ||
---|---|---|---|
AISI 347 | Bar | AISI 347 | |
DIN 1.4044 | Bar | DIN 1.4044 | |
DIN 1.4534 | Sheet | DIN 1.4534 | |
DIN 1.6354 | Bar | DIN 1.6354 | |
EN 1.4545 | Sheet | EN 1.4545 | AMS 5659 |
UNS K93120 | Sheet | UNS K93120 | AMS 6514 |
UNS S13800 | Sheet | UNS S13800 | AMS 5629 |
UNS S17400 | Bar | UNS S17400 | AMS 5662, AMS 5643 |
UNS S34700 | Bar | UNS S34700 | AMS 5646 |