Aisha Steel Mills Limited (ASML) is a Group Company of Arif Habib. ASML is a state of the art cold rolling & hot dipped galvanized rolling complex with an overall capacity of 700,000 metric tons per annum.ASML is one of the largest private sector investments in the value added flat-rolled steel industry in Pakistan.
Sede
Karachi, Pakistan
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
, ISO 14001
Grade | Shape | ||
---|---|---|---|
EN DC01 | Coil, Sheet | EN DC01 | JIS G3141, ASTM A1008 |
EN DC04 | Coil, Sheet | EN DC04 | JIS G3141, ASTM A1008 |
EN DX51D | Coil, Sheet | EN DX51D | JIS G3302, ASTM A653 |
JIS SGCC | Coil, Sheet | JIS SGCC | JIS G3302, ASTM A653 |
JIS SGCD1 | Coil, Sheet | JIS SGCD1 | JIS G3302, ASTM A653 |
JIS SGCH | Coil, Sheet | JIS SGCH | JIS G3302, ASTM A653 |
JIS SPCC | Coil, Sheet | JIS SPCC | JIS G3141, ASTM A1008 |
JIS SPCD | Coil, Sheet | JIS SPCD | JIS G3141, ASTM A1008 |
JIS SPCE | Coil, Sheet | JIS SPCE | JIS G3141, ASTM A1008 |
JIS SPCG | Coil, Sheet | JIS SPCG | JIS G3141, ASTM A1008 |