Aurubis has produced copper and other metals that are crucial for modernization and for the ongoing development of our lives over the next decades. As a result, the company considers itself a real multimetal provider.
Sede
Hamburg, Germany
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 14001
, ISO 45001
, ISO 9001
, ISO 50001
Grade | Shape | ||
---|---|---|---|
BE 58 | Forging, Strip, Foil, Plate, Tube, Profile | EN Cu-PHC, EN Cu-HCP, UNS C10300, EN CR020A, EN CR021A | ASTM B379 |
BG35 | Forging, Strip, Foil, Plate, Tube, Profile, Bar | EN CuAg0.04, EN CuAg0.1, UNS C10400, UNS C10700, EN CR014A, EN CR016A | ASTM B152 |
DHP | Forging, Strip, Foil, Plate, Tube, Profile | EN Cu-DHP, UNS C12200, EN CR024A | ASTM B379 |
DIN 2.1202 | Rod | DIN 2.1202, EN CR017, EN CR019A, UNS C11300, UNS C11600 | DIN EN 1977, ASTM B49 |
DLP | Forging, Strip, Foil, Plate, Tube, Profile | EN Cu-DLP, UNS C12000, EN CR023A | ASTM B379 |
EN Cu-DXP | Rod | EN Cu-DXP, EN CR025A, UNS C12200 | DIN EN 1977, ASTM B49 |
EN Cu-ETP | Rod | EN Cu-ETP, EN CW003A, UNS C11040 | DIN EN 1977, ASTM B49 |
EN Cu-HCP | Rod | EN Cu-HCP, EN CW021A, R021, EN CR022A, UNS C10300 | DIN EN 1977, ASTM B49 |
EN Cu-OFE | Rod | EN Cu-OFE, UNS C10100, EN CR009A, JIS C1011 | DIN EN 1977, ASTM B49 |
EN Cu64ZnNi3 | Strip | EN Cu64ZnNi3, UNS C74400 | |