AW Fraser produces and supplies, continuous cast and centrifugally cast bronze bars; hollow and solid brass extrusions; and, precision machined components from a variety of bronze and brass alloys.
Sede
Christchurch, Canterbury, New Zealand
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 14001
, ISO 9001
Grade | Shape | ||
---|---|---|---|
Alloy LB2 | Casting, Bar | UNS C93700, EN CC495K, DIN 2.1176, EN CuPb10Sn, JIS CAC603C, UNI 7013-72-3A | ASTM B505 |
Alloy LB4 | Casting, Bar | UNS C93500, EN CC494K, EN CuSn5Pb9 | ASTM B505 |
Alloy LG1 | Casting, Bar | UNS C84400, EN CC490K, DIN 2.1098, EN CuSn2ZnPb, JIS CAC401 | ASTM B505 |
Alloy LG2 | Casting, Bar | UNS C83600, EN CC491K, DIN 2.0196, EN CuSn5ZnPb, JIS CAC402C, UNI 7013-72-8A | ASTM B271, ASTM B505 |
Alloy LG54 | Casting, Bar | UNI 5275, UNS C95500, EN CC333G, DIN 2.0981, EN CuAl11Ni, JIS CAC703, BS AB2 | ASTM B271, ASTM B505 |
Alloy PB1 | Casting, Bar | UNS C90700, EN CC481K, DIN 2.1050, EN CuSn10, JIS CAC502C | ASTM B505 |
Alloy PB2 | Casting, Bar | UNS C90800, EN CC483K, DIN 2.1052, EN CuSn12, JIS CAC502C, UNI 7013-72-2A | AS 1565 |
EN CuAl10Ni5Fe5 | Casting, Bar | EN CuAl10Ni5Fe5, EN CC333G | BS EN 1982 |
EN CuZn34Al2 | Casting, Bar | EN CuZn34Al2 | BS EN 1982 |
UNS C35330 | Casting, Bar | UNS C35330, EN CW602N, DIN 2.0371, EN CuZn36Pb3, BS CZ132 | AS/NZS 1567 |