Cubex Tubings Limited manufactures copper alloy tubes, wires, sheets, flats, and rods for boilers, condensers, heat exchangers, medical purposes, infrastructure, power generation, defense, and many other processes. Our factory is strategically located to expedite the delivery of our products to shipping ports across the world.
Sede
Hyderabad,Telangana, India
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
EN Cu-DLP | Tube | EN Cu-DLP | |
EN Cu-ETP | Tube | EN Cu-ETP | |
UNS C12200 | Tube | UNS C12200, EN Cu-DHP | ASTM B75, ASTM B111, ASTM B395, ASME SB111, ASME SB395 |
UNS C44300 | Tube | UNS C44300, DIN CuZn28Sn1 | ASTM B111, ASTM B395, ASME SB111, ASME SB395 |
UNS C68700 | Tube | UNS C68700, BS CZ110, DIN CuZn22AI2 | ASTM B111, ASTM B395, ASME SB111, ASME SB395 |
UNS C70600 | Tube | UNS C70600, BS CN102, DIN CuNi10Fe1Mn | ASTM B111, ASTM B395, ASTM B466, ASME SB111, ASME SB395, ASME SB466 |
UNS C71500 | Tube | UNS C71500, BS CN107, DIN CuNi30Mn1Fe | ASTM B111, ASTM B395, ASTM B466, ASTM B467, ASTM B543, ASME SB111, ASME SB395, ASME SB466 |
UNS N04400 | Tube | UNS N04400, Alloy 400 | ASTM B163, ASTM B165, ASME SB163, ASME SB165 |