Welcome to City Special Metals Ltd. We’re a globally recognised stockist of low & controlled expansion alloys, including: Invar 36, Kovar & Alloy 42.Our team is dedicated to delivering high quality, fully certified alloys from a UK stock inventory of unrivalled size. This dedication has followed us since establishment in 2001 and contributed to us achieving our AS9120/ISO9001 Quality Management System accreditation, held since 2015.We have experience working in a vast range of market sectors and we’re confident in our ability to deliver. Our team will work with you to deliver bespoke speciality metals for any requirement.
Sede
Benfleet, United Kingdom
Sitio web
Tipo
Distribuidor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
17-4 PH | Plate, Bar, Sheet | 17-4 PH, UNS S17400, AISI 630 | ASTM A564 |
Alloy 200 | Bar, Plate, Sheet | Alloy 200 | |
Alloy 201 | Bar, Plate, Sheet | Alloy 201 | |
Alloy 42 | Bar, Sheet, Coil | Alloy 42 | |
Inconel 625 | Bar, Sheet, Coil | Inconel 625, Alloy 625 | ASTM B443, B446, DIN 17744, ISO 15156-3, NACE MR0175 |
Inconel 718 | Bar, Plate, Sheet | Inconel 718, Alloy 718, UNS N07718, EN 2.4668 | ASTM B637 |
Invar 36 | Plate, Bar, Sheet, Coil, Wire | Invar 36 | |