Energy Alloys Global Solutions is one of the largest global providers of in-house value-added manufacturing and distribution solutions for tube and bar products to the oil and gas industry.
Sede
Houston,Texas, United States
Sitio web
Tipo
Manufacturer, Processor and Distributor
Grade | Shape | ||
---|---|---|---|
AISI 1018 | Bar | AISI 1018 | ASTM A29, ASTM A108, API 6A |
AISI 1026 | Bar, Tube | AISI 1026 | ASTM A29, ASTM A108, API 6A |
AISI 1045 | Bar | AISI 1045 | ASTM A29, ASTM A108, API 6A |
AISI 304 | Bar | AISI 304 | ASTM A276 |
AISI 304L | Bar | AISI 304L | ASTM A276 |
AISI 316 | Bar | AISI 316 | ASTM A276 |
AISI 316L | Bar | AISI 316L | ASTM A276 |
AISI 410 | Bar | AISI 410 | ASTM A276, API 6A |
AISI 4130 | Bar, Tube | AISI 4130 | ASTM A29, ASTM A519, API 6A |
AISI 4145 mod. | Bar | AISI 4145 mod., AISI 4145H | ASTM A29, API 7-1, API 14A |