EZM Edelstahlzieherei Mark GmbH is a manufacturer and international operating supplier of bright steel and profiles made of steel and titanium, focusing on applications in automotive engineering, machine construction, energy engineering and medical equipment.
Sede
Wetter,North Rhine-Westphalia, Germany
Sitio web
Tipo
Manufacturer, Processor and Distributor
Certifications
IATF 16949
, ISO 9001
, ISO 14001
Grade | Shape | ||
---|---|---|---|
CoCr28Mo | Bar, Profile | CoCr28Mo | ISO 5832-12, ASTM F1537 |
DIN 3.7025 | Wire, Bar, Sheet | DIN 3.7025, UNS R50250 | ISO 5832-2, ASTM F67 |
DIN 3.7035 | Wire, Bar, Sheet | DIN 3.7035, UNS R50400 | ISO 5832-2, ASTM F67 |
DIN 3.7055 | Wire, Bar, Sheet | DIN 3.7055, UNS R50550 | ISO 5832-2, ASTM F67 |
DIN 3.7065 | Wire, Bar, Sheet | DIN 3.7065, UNS R50700 | ISO 5832-2, ASTM F67 |
DIN 3.7165 | Wire, Bar, Sheet | DIN 3.7165, UNS R56401, Ti-6Al-4V (ELI), Titanium Grade 5 | ISO 5832-3, ASTM F136 |
EN 1.2791 | Bar, Profile | EN 1.2791 | |
EN 1.3910 | Bar, Profile | EN 1.3910 | |
EN 1.3965 | Bar, Profile | EN 1.3965 | |
EN 1.4021 | Wire, Bar, Sheet | EN 1.4021, AISI 420A, UNS S42000, ER218 | ASTM A193, ASTM A194, ASTM A276, ASTM A479, ASTM F899, AMS 5848, ASTM A240, ASTM A182, AWS A5.9 |