THE WORLD-WIDE SPECIALIST COPPER CONDUCTOR MANUFACTURER FOR ELECTRICAL EQUIPMENT.From the copper bar to the most sophisticated copper component, (flat, round, square copper bars, profiles and components).
Sede
PONT DE CHÉRUY, France
Sitio web
Tipo
Fabricante
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
EN Cu-ETP | Bar, Coil, Wire | EN Cu-ETP, EN CW004A | |
EN Cu-HCP | Bar, Coil, Wire | EN Cu-HCP, EN CW021A | |
EN Cu-OF | Bar, Coil, Wire | EN Cu-OF, EN CW008A | |
EN Cu-PHC | Bar, Coil, Wire | EN Cu-PHC, EN CW020A | |
EN CuAg0.04 | Bar, Coil, Wire | EN CuAg0.04, EN CW011A | |
EN CuAg0.04P | Bar, Coil, Wire | EN CuAg0.04P, EN CW014A | |
EN CuAg0.07 | Bar, Coil, Wire | EN CuAg0.07, EN CW012A | |
EN CuAg0.07P | Bar, Coil, Wire | EN CuAg0.07P, EN CW015A | |
EN CuAg0.10 | Bar, Coil, Wire | EN CuAg0.10, EN CW013A | |
EN CuAg0.1P | Bar, Coil, Wire | EN CuAg0.1P, EN CW016A | |