We offer distribution and production of bar, sheet, plate, forgings, and fasteners. See our Linecard Of Alloys And Sizes. Stocking: Hastelloy®, Inconel®, Monel®, Nitronic®, Cobalt based alloys such as Stellite®, and L605, and commercially Pure Nickel grades 200/201.
Sede
Tipton,Indiana, United States
Sitio web
Tipo
Manufacturer, Processor and Distributor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
Alloy 200 | Bar, Sheet, Plate, Tube, Pipe, Fitting, Forging, Weld Wire, Weld Electrode | Alloy 200, UNS N02200, DIN 2.4066 | ASTM B160, DIN 17752, BS 3076, ASTM B162, DIN 17750, BS 3072, ASTM B622, ASTM B161, ASTM B163, DIN 17740, BS 3074, ASTM B366, ASTM B564 |
Alloy 201 | Bar, Sheet, Plate, Fitting, Forging, Weld Electrode | Alloy 201, UNS N02201, DIN 2.4068 | ASTM B160, DIN 17752, BS 3076, ASTM B162, DIN 17750, BS 3072, ASTM B366, ASTM B564, DIN 17754 |
Carpenter 20Cb-3 | Bar, Wire, Sheet, Plate, Fitting, Forging, Weld Wire, Weld Electrode | Carpenter 20Cb-3, UNS N08020 | ASTM B473, ASTM B471, ASTM B463, ASTM B366, ASTM B462, E320LR |
FerrAlium 255 | Bar, Plate, Sheet, Weld Electrode | FerrAlium 255, UNS S32550, DIN 1.4507 | ASTM A479, ASTM A240 |
Hastelloy B-2 | Bar, Sheet, Plate, Fitting, Forging, Weld Wire, Weld Electrode, Pipe, Tube, Rod | Hastelloy B-2, UNS N10665, DIN 2.4617, AWS ERNiMo7 | ASTM B333, ASME SB333, ASTM B335, ASME SB335, ASTM B366, ASME SB366, ASTM B564, AWS A5.14, AWS A5.11, ASTM B622, ASME SB622, ASTM B619, ASME SB619, ASTM B626, ASME SB626 |
Hastelloy C-22 | Bar, Sheet, Plate, Forging, Fitting | Hastelloy C-22, UNS N06022 | ASTM B574, ASTM B575, ASME SB366, ASME SB564 |
Hastelloy C-276 | Bar, Sheet, Plate, Forging, Fitting, Tube, Pipe, Weld Wire, Weld Electrode | Hastelloy C-276, UNS N10276, DIN 2.4819, AWS ERNiCrMo4 | ASTM B574, DIN 17752, ASTM B575, DIN 17750, ASTM B366, ASTM B564, ASTM B619, ASTM B622, ASTM B626, DIN 17751, AWS A5.14, AWS A5.11 |
Hastelloy X | Bar, Wire, Sheet, Plate, Tube, Pipe, Fitting, Forging, Weld Wire, Weld Electrode | Hastelloy X, Hastelloy HX, UNS N06002, DIN 2.4665, ERNiCrMo2 | ASTM B572, AMS 5754, AMS 5798W, AMS 5798C, ASTM B435, AMS 5536, AMS 5587, AMS 5588, ASTM B619, ASTM B622, ASTM B366, GE B50TF31, AWS A5.14, AWS A5.11 |
Haynes 25 | Bar, Sheet, Plate, Foil, Tube, Forging, Weld Wire | Haynes 25, Alloy L-605, UNS R30605, DIN 2.4964 | AMS 5759, ASTM F90, GE B50T26A, MCI 1031, GPS 2051, AMS 5537 |
Incoloy 27-7Mo | Bar, Wire, Sheet, Plate, Tube, Pipe, Fitting, Forging | Incoloy 27-7Mo, UNS S31277 | ASTM A479, ASME SA479, ASTM A240, ASME SA240, ASTM A213, ASME SA213, ASTM A249, ASME SA249, ASTM A312, ASME SA312, ASTM A182 |