We develop and produce high quality and durable profile systems from steel and stainless steel, aluminum and other materials. Areas of application are e.g. B. Elements of transport trolleys in mechanical engineering, housing systems for battery systems and much more. IsoProfil always guarantees 100% functionality - all components are coordinated with one another and together form a perfect system.
Sede
Wuppertal,North Rhine-Westphalia, Germany
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
ASW 205 | Profile | DIN AlMgSi0.5 | DIN EN 12020-2, DIN EN 755-9 |
ASW 209 | Profile | DIN AlSiMg(A) | DIN EN 12020-2, DIN EN 755-9 |
ASW 210 | Profile | DIN AlSi1MgMn | DIN EN 12020-2, DIN EN 755-9 |
ASW 220 | Profile | DIN AlCu4Mg1 | DIN EN 12020-2, DIN EN 755-9 |
ASW 510 | Profile | DIN AlZnMgCu1.5 | DIN EN 12020-2, DIN EN 755-9 |
KSW 004 | Profile | EN Cu-ETP, EN CW004A | DIN EN 12167, DIN EN 12165 |
KSW 008 | Profile | EN Cu-OF, EN CW008A | DIN EN 12167, DIN EN 12165 |
KSW 024 | Profile | EN Cu-DHP, EN CW024A | DIN EN 12167, DIN EN 12165 |
MSW 055 | Profile | EN CuZn43Pb2Al, DIN Ms56 | DIN EN 12167, DIN EN 12615 |
MSW 057 | Profile | EN CuZn39Pb3, DIN Ms58 | DIN EN 12167, DIN EN 12615 |