Eaton Steel Bar Company (ESBC) is more than just a steel bar company. The highest quality hot rolled and cold drawn bars supply the foundation of our business, but we also solve your steel bar supply chain problems. With over 300 team members working together at Eaton Steel, we ensure that our customers are given the simplest, most cost effective solution to any problem.
Sede
Oak Park,Michigan, United States
Sitio web
Tipo
Processor and Distributor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
AISI 1018 | Bar | AISI 1018 | ASTM A29, ASTM A576 |
AISI 1020 | Bar | AISI 1020 | |
AISI 1045 | Bar | AISI 1045 | ASTM A29, ASTM A576 |
AISI 1141 | Bar | AISI 1141 | |
AISI 1144 | Bar | AISI 1144 | ASTM A29, ASTM A576 |
AISI 1541 | Bar | AISI 1541 | ASTM A29, ASTM A576 |
AISI 4140 | Bar | AISI 4140 | |
AISI 4150 | Bar | AISI 4150 | ASTM A29, ASTM A322 |
AISI 4340 | Bar | AISI 4340 | ASTM A108, ASTM A322 |
AISI 8620 | Bar | AISI 8620 | ASTM A108, ASTM A322 |