Mannesmann Precision Tubes is a leading manufacturer of cold drawn seamless and welded precision steel tubes as well as seamless, hot-finished tubes.
Sede
Mülheim an der Ruhr,North Rhine-Westphalia, Germany
Tipo
Fabricante y procesador
Certifications
ISO 9001
, IATF 16949
, ISO 14001
, ISO 50001
, ISO 45001
Grade | Shape | ||
---|---|---|---|
EN 100Cr6 | Tube | EN 100Cr6 | EN 10210-1, EN 10216-1, EN 10216-2, EN 10216-3, EN 10216-4, EN 10255, EN 10294, EN 10297, EN ISO 3183, API 5L, API 5CT, ASTM A519, ASTM A106, ASTM A192, ASTM A210, ASTM A213 |
EN 16MnCr5 | Tube | EN 16MnCr5 | EN 10305-1, EN 10305-4 |
EN 20MnCr5 | Tube | EN 20MnCr5 | EN 10305-1, EN 10305-4 |
EN 20MoCr4 | Tube | EN 20MoCr4 | EN 10305-1, EN 10305-4 |
EN 22MnB5 | Tube | EN 22MnB5 | EN 10305-1, EN 10305-4, EN 10305-2, EN 10305-3, EN 10210-1, EN 10216-1, EN 10216-2, EN 10216-3, EN 10216-4, EN 10255, EN 10294, EN 10297, EN ISO 3183, API 5L, API 5CT, ASTM A519, ASTM A106, ASTM A192, ASTM A210, ASTM A213 |
EN 25CrMo4 | Tube | EN 25CrMo4 | EN 10305-1, EN 10305-4, EN 10210-1, EN 10216-1, EN 10216-2, EN 10216-3, EN 10216-4, EN 10255, EN 10294, EN 10297, EN ISO 3183, API 5L, API 5CT, ASTM A519, ASTM A106, ASTM A192, ASTM A210, ASTM A213 |
EN 26MnB5 | Tube | EN 26MnB5 | EN 10305-1, EN 10305-4, EN 10305-2, EN 10305-3, EN 10210-1, EN 10216-1, EN 10216-2, EN 10216-3, EN 10216-4, EN 10255, EN 10294, EN 10297, EN ISO 3183, API 5L, API 5CT, ASTM A519, ASTM A106, ASTM A192, ASTM A210, ASTM A213 |
EN 34CrMo4 | Tube | EN 34CrMo4 | EN 10305-1, EN 10305-4, EN 10210-1, EN 10216-1, EN 10216-2, EN 10216-3, EN 10216-4, EN 10255, EN 10294, EN 10297, EN ISO 3183, API 5L, API 5CT, ASTM A519, ASTM A106, ASTM A192, ASTM A210, ASTM A213 |
EN 34MnB5 | Tube | EN 34MnB5 | EN 10305-1, EN 10305-4, EN 10305-2, EN 10305-3, EN 10210-1, EN 10216-1, EN 10216-2, EN 10216-3, EN 10216-4, EN 10255, EN 10294, EN 10297, EN ISO 3183, API 5L, API 5CT, ASTM A519, ASTM A106, ASTM A192, ASTM A210, ASTM A213 |
EN 42CrMo4 | Tube | EN 42CrMo4 | EN 10305-1, EN 10305-4, EN 10210-1, EN 10216-1, EN 10216-2, EN 10216-3, EN 10216-4, EN 10255, EN 10294, EN 10297, EN ISO 3183, API 5L, API 5CT, ASTM A519, ASTM A106, ASTM A192, ASTM A210, ASTM A213 |