METRA Industry produces high technological content aluminium extrusions through a vertically integrated supply chain that guarantees the quality of the entire productive process and of the finished product to respond to the complex needs of numerous end markets.
Sede
Rodengo Saiano,Brescia, Italy
Sitio web
Tipo
Manufacturer, Processor and Distributor
Certifications
ISO 3834-2
, ISO 9001
, ISO 22163
, IATF 16949
, EN 15085-2
, ISO 14001
Grade | Shape | ||
---|---|---|---|
EN AW-3103 | Profile, Beam, Pipe, Bar | EN AW-3103 | EN 573-3, EN 755-2 |
EN AW-6005A | Profile, Pipe, Bar | EN AW-6005A | EN 573-3, EN 755-2 |
EN AW-6060 | Profile, Beam, Pipe, Bar | EN AW-6060 | EN 573-3, EN 755-2 |
EN AW-6061 | Profile, Pipe, Bar | EN AW-6061 | EN 573-3, EN 755-2 |
EN AW-6063 | Profile, Beam, Pipe, Bar | EN AW-6063 | EN 573-3, EN 755-2 |
EN AW-6082 | Profile, Pipe, Bar | EN AW-6082 | EN 573-3, EN 755-2 |
EN AW-6160 | Profile, Pipe, Bar | EN AW-6160 | EN 573-3, EN 755-2 |