Through the merger with FERRIT Blechservice GmbH & Co. KG in 2020, we have significantly expanded our portfolio to include the area of production with an extensive range of machinery. This step offers our customers even more flexibility and the possibility to optimally support them in the development and implementation of projects.
Sede
Rosengarten, Germany
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
AISI 301 | Sheet, Coil, Strip, Profile | AISI 301, UNS S30100, EN 1.4310 | |
AISI 303 | Sheet, Profile, Bar | AISI 303, UNS S30300, EN 1.4305 | |
AISI 304 | Sheet, Coil, Strip, Profile, Bar, Tube | AISI 304, UNS S30400, EN 1.4301 | |
AISI 304H | Sheet, Coil, Strip, Profile, Tube | AISI 304H, UNS S30409, EN 1.4948 | |
AISI 304L | Sheet, Coil, Strip, Profile, Bar, Tube | AISI 304L, UNS S30403, EN 1.4307, EN 1.4306 | |
AISI 309 | Sheet, Coil, Strip, Profile, Bar, Tube | AISI 309, UNS S30900, EN 1.4828 | |
AISI 309S | Sheet, Coil, Strip, Profile, Bar, Tube | AISI 309S, UNS S30908, EN 1.4833 | |
AISI 310 | Sheet, Coil, Strip, Profile, Bar, Tube | AISI 310, UNS S31000, EN 1.4841 | |
AISI 310S | Sheet, Coil, Strip, Profile, Bar, Tube | AISI 310S, UNS S31008, EN 1.4845 | |
AISI 316 | Sheet, Coil, Strip, Profile, Bar | AISI 316, UNS S31600, EN 1.4436 | |