Nippon Steel Corporation Group will pursue world-leading technologies and manufacturing capabilities, and contribute to society by providing excellent products and services.
Sede
Tokyo, Japan
Sitio web
Tipo
Manufacturer, Processor and Distributor
Certifications
ISO 9001
, ISO 14001
Grade | Shape | ||
---|---|---|---|
AISI 301 | Strip, Sheet, Plate, Bar, Forging | JIS SUS301 | JIS G4304, JIS G4305, JIS G4312 |
AISI 301L | Strip, Sheet, Plate, Bar, Forging | JIS SUS301L | JIS G4304, JIS G4305, JIS G4312 |
AISI 301N | Strip, Sheet, Plate, Bar, Forging | JIS SUS301 | JIS G4304, JIS G4305, JIS G4312 |
AISI 303 | Strip, Sheet, Plate, Bar, Forging | JIS SUS303 | JIS G4304, JIS G4305, JIS G4312 |
AISI 304 | Strip, Sheet, Plate, Bar, Forging | JIS SUS304 | JIS G4304, JIS G4305, JIS G4312 |
AISI 304L | Strip, Sheet, Plate, Bar, Forging | JIS SUS304L | JIS G4304, JIS G4305, JIS G4312 |
AISI 304MK | Bar, Plate, Forging | JIS SUS304J2 | JIS G4304, JIS G4305, JIS G4312 |
AISI 304N2 | Strip, Sheet, Plate, Bar, Forging | JIS SUS304N2 | JIS G4304, JIS G4305, JIS G4312 |
AISI 305 | Strip, Sheet, Plate, Bar, Forging | JIS SUS305 | JIS G4304, JIS G4305, JIS G4312 |
AISI 309S | Strip, Sheet, Plate, Bar, Forging | JIS SUS309S | JIS G4304, JIS G4305, JIS G4312 |