We manufacture extruded, forged and ring-rolled products of Aluminium, Magne¬sium, Copper, Titanium and Nickel alloys for customers who require safety, lightweight design, reliability and durability.
Sede
Meinerzhagen, Germany
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
, ISO 14001
, ISO 45001
, ISO 5001
, ISO 50001
, ISO 27001
, IEC 27001
, IATF 16949
, EN 9100
, ISO 22163
, AD 2000
Grade | Shape | ||
---|---|---|---|
DIN AlCu2Mg1.5Ni | Pipe, Bar, Profile | DIN AlCu2Mg1.5Ni, EN AW-2618A | DIN EN 573 |
DIN AlCu4Mg1 | Pipe, Bar, Profile | DIN AlCu4Mg1, EN AW-2024 | DIN EN 573 |
DIN AlCu4SiMg | Pipe, Bar, Profile | DIN AlCu4SiMg, EN AW-2014, EN AW-2014A | DIN EN 573 |
DIN AlMg0.7Si | Pipe, Bar, Profile | DIN AlMg0.7Si, EN AW-6063 | DIN EN 573 |
DIN AlMg0.9Si0.9MnCu(A) | Pipe, Bar, Profile | DIN AlMg0.9Si0.9MnCu(A), EN AW-6110A | DIN EN 573 |
DIN AlSi1MgMn | Pipe, Bar, Profile | DIN AlSi1MgMn, EN AW-6082 | DIN EN 573 |
DIN AlZn4.5Mg1 | Pipe, Bar, Profile, Wire | DIN AlZn4.5Mg1, EN AW-7020 | DIN EN 573 |
DIN AlZn5.5MgCu | Pipe, Bar, Profile | DIN AlZn5.5MgCu, EN AW-7075, EN AW-7175, EN AW-7475 | DIN EN 573 |
DIN AlZn5Mg1Zr | Pipe, Bar, Profile, Wire | DIN AlZn5Mg1Zr, EN AW-7108A | DIN EN 573 |
DIN AlZn6CuMgZr | Pipe, Bar, Profile | DIN AlZn6CuMgZr, EN AW-7050 | DIN EN 573 |