Grade | Shape | ||
---|---|---|---|
EN 100CrMnSi4-4 | Bar, Ring | EN 100CrMnSi4-4, ASTM A485 B2 | EN ISO 683-17, ASTM A485 |
EN 16MnCr5 | Bar | EN 16MnCr5, EN 20MnCr5 | |
EN 16NiCrS4 | Bar | EN 16NiCrS4 | |
EN 18CrNiMo7-6 | Bar | EN 18CrNiMo7-6, DIN 1.6587, AISI 4820, DIN 17CrNiMo6, AFNOR 18CND6 | EN ISO 683-3, EN ISO 683-17 |
EN 20NiCrMo2-2 | Bar | EN 20NiCrMo2-2, SAE 8620, BS 805H22, AFNOR 20NCD2, SS 2506 | |
EN C15E | Bar | EN C15E | |
Ovaco 677 | Bar | EN 67SiMnCrMo6-6-4, EN 66SiMnCrMo6-6-4 | |
Ovako 124 | Tube | EN 20MoCr4 | EN 10084 |
Ovako 146 | Bar | EN 16NiCrMo7-8 | |
Ovako 152 | Bar | EN 20NiCrMo2-2, AISI 8620, AISI 8620H, DIN 1.6522, DIN 1.6523, DIN 1.6526, SS 2506, UNS H86200 | EN ISO 683-3 |