Grade | Shape | ||
---|---|---|---|
Anticorodal 100/112 | Bar | EN AW-6082, DIN AlSi1MgMn, DIN AlMgSi1, DIN 3.2315 | DIN EN 573-3, DIN EN 754-2, DIN EN 754-3, DIN EN 755-2, DIN EN 755-3, DIN EN 515 |
Decoltal 500 / Aludur D202 | Bar | EN AW-2011, EN AlCu6BiPb, DIN AlCuBiPb, EN AW-2030, DIN AlCu4PbMg, DIN AlCuMgPb, DIN 3.1655 | DIN EN 573-3, DIN EN 754-2, DIN EN 754-3, DIN EN 755-2, DIN EN 755-3, DIN EN 515 |
EN AW-1050A | Wire | EN AW-1050A, DIN Al99.5, DIN 3.0255 | DIN EN 573-3, DIN EN 1301-2, DIN EN 1301-3 |
EN AW-2030 | Bar | EN AW-2030, DIN AlCu4PbMg, AA 6026 | |
EN AW-6026 | Bar | EN AW-6026 | DIN EN 573-3, DIN EN 754-2, DIN EN 754-3, DIN EN 755-2, DIN EN 755-3 |
EN AW-6082 | Bar | EN AW-6082, DIN AlSi1MgMn, DIN AlMgSi1 | DIN EN 573-3, DIN EN 754-2, DIN EN 754-4, DIN EN 755-2, DIN EN 755-4, DIN EN 515 |
EN CC483K | Bar | EN CC483K, EN CuSn12, DIN 2.1052, DIN G-CuSn12 | DIN EN 1982 |
EN CC493K | Bar, Tube | EN CC493K, EN CuSn7Zn4Pb7, DIN 2.1090, DIN G-CuSn7ZnPb | DIN EN 1982 |
EN CC496K | Bar | EN CC496K, EN CuSn7Pb15, EN CuPb15Sn, DIN 2.1182, DIN G-CuPb15Sn | DIN EN 1982 |
EN CuNi7Zn39Pb3Mn2 | Bar | EN CW400J, EN CuNi7Zn39Pb3Mn2, DIN 2.0771 | DIN EN 12164 |