Specialized in the production of steel for all industrial uses, Rodacciai has always distinguished itself through a unique production philosophy: the choice to have, just a few years after its foundation, its own rolling mill.
Sede
Bosisio Parini LC, Italy
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
, EC 1907
, EC 1272
, ISO 14001
, BS 6744
, EN 12074
Grade | Shape | ||
---|---|---|---|
EN 100Cr6 | Bar, Coil | EN 1.3505, UNI 100Cr6, DIN 100Cr6, DIN 1.3505, AFNOR 100C6, BS 2S135, EN 100Cr6 | EN ISO 683-17, UNI 3097, DIN 17230, NFA 35-565, BS 970-3, ASTM A29 |
EN 10SPb20 | Bar, Coil | EN 1.0722, UNI CF10SPb20, DIN 10SPb20, DIN 1.0722, AFNOR 13MF4, SAE 11L09, EN 10SPb20 | EN ISO 683-4, EN 10277, EN 10087, EN 10277-3, UNI 4838, DIN 1651, NFA 35-562, BS 970-3, ASTM A29 |
EN 11SMn30 | Bar, Coil | EN 1.0715, UNI CF9SMn28, DIN 9SMn28, DIN 1.0715, AFNOR S250, BS 230M07, EN 11SMn30 | EN ISO 682-4, EN 10277, EN 10087, EN 10277-3, UNI 4838, DIN 1651, NFA 35-561, BS 970-3, ASTM A29 |
EN 11SMn37 | Bar, Coil | EN 1.0736, UNI CF9SMn36, DIN 9SMn36, DIN 1.0736, AFNOR S300, EN 11SMn37 | EN ISO 683-4, EN 10277, EN 10087, EN 10277-3, UNI 4838, DIN 1651, NFA 35-561, BS 970-3, ASTM A29 |
EN 11SMnPb30 | Bar, Coil | EN 1.0718, UNI CF9SMnPb28, DIN 9SMnPb28, DIN 1.0718, AFNOR S250Pb, BS 230M07, SAE 12L14, EN 11SMnPb30 | EN ISO 683-4, EN 10277, EN 10087, EN 10277-3, UNI 4838, DIN 1651, NFA 35-561, BS 970-3, ASTM A29 |
EN 11SMnPb30+Te+Bi | Bar, Coil | EN 1.0718, UNI CF9SMnPb28, DIN 9SMnPb28, DIN 1.0718, AFNOR S250Pb, SAE 12L14, EN 11SMnPb30TeBi | EN ISO 683-4, EN 10277, EN 10087, EN 10277-3, UNI 4838, DIN 1651, NFA 35-561, BS 970-3, ASTM A29 |
EN 11SMnPb37 | Bar, Coil | EN 1.0737, UNI CF9SMnPb36, DIN 9SMnPb36, DIN 1.0737, AFNOR S300Pb, EN 11SMnPb37 | EN ISO 683-4, EN 10277, EN 10087, EN 10277-3, UNI 4838, DIN 1651, NFA 35-561, BS 970-3, ASTM A29 |
EN 11SMnPb37+Te+Bi | Bar, Coil | EN 1.0737, UNI CF9SMnPb36, DIN 9SMnPb36, DIN 1.0737, AFNOR S300Pb, SAE 12L14, EN 11SMnPb37TeBi | EN ISO 683-4, EN 10277, EN 10087, EN 10277-3, UNI 4838, DIN 1651, NFA 35-561, BS 970-3, ASTM A29 |
EN 15NiCr13 | Bar, Coil | EN 1.5752, UNI 16NiCr11, AFNOR 14NC11, EN 15NiCr13 | EN 10084, EN 10277-4, UNI 5331, DIN 17210, NFA 35-551, BS 970-3, ASTM A29 |
EN 15SMn13 | Bar, Coil | EN 1.0725, DIN 15S10, DIN 1.0725, BS 214M15, SAE 1117, EN 15SMn13 | EN ISO 683-4, EN 10277, ASTM A29, SAE J403, EN 10087, EN 10277-3, UNI 4838, DIN 1651, NFA 35-562, BS 970-3 |