Metal and Mineral (except Petroleum) Merchant Wholesalers Industry.
Sede
Temperance,Michigan, United States
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
, AS 9100D
Grade | Shape | ||
---|---|---|---|
13-8 PH | Bar | EN 1.4548, UNS S13800, DIN 1.4548 | AMS 5629, ASTM A564 |
15-5 PH | Plate, Bar | UNS S15500, EN 1.4545, ASTM XM-12 | AMS 5659, AMS 5862J, ASME SA564, ASME SA693, ASME SA705, ASTM A564, ASTM A693, ASTM A698, ASTM A705, BAC 5439 Rev H Class A Type1, Boeing BMS 7-240, BSS 7055, STD 2154 |
17-4 PH | Plate, Bar | EN 1.4548, UNS S17400, DIN 1.4548 | AMS 5604, AMS 5643, AMS 5825, ASME SA564, ASME SA693, ASME SA705, ASTM A564, ASTM A693, ASTM A705, ISO 15156-3, NACE MR 0175 |
AISI 303 | Bar | UNS S30300, DIN 1.4305 | AMS 5640, ASTM A262, ASTM A314, ASTM A484, ASTM A582 |
AISI 304 | Plate, Weld Wire | EN 1.4948, AISI 304H | AMS 5513, ASME SA240, ASTM A240, ASTM A959 |
AISI 309 | Plate, Rod, Coil, Pipe, Bar, Sheet | EN 1.4828, EN 1.4833, UNS S30908, UNS S30909, DIN 1.4833 | AMS 5523, ASME SA240, ASME SA312, ASME SA479, ASTM A240, ASTM A276, ASTM A312, ASTM A479 |
AISI 310 | Flange, Plate, Rod, Coil, Pipe, Tube, Bar, Sheet | UNS S31008, UNS S31009, DIN 1.4845 | AMS 5521, AMS 5651, ASME SA240, ASME SA312, ASME SA479, ASTM A240, ASTM A276, ASTM A312, ASTM A479, EN 10095 |
AISI 317L | Plate | UNS S31703, EN 1.4438 | ASME SA240, ASTM A240 |
AISI 321 | Plate, Pipe, Bar, Sheet | EN 1.4541, UNS S32100, DIN 1.4541 | AMS 5510, AMS 5645, ASME SA240, ASME SA312, ASME SA479, ASTM A240, ASTM A276, ASTM A312, ASTM A479, AMS QQ-S-763, AMS QQ-S-766 |
AISI 347 | Plate, Bar, Sheet | UNS S34700, UNS S34709, EN 1.4550 | AMS 5512, AMS 5646, AMS 5680, ASME SA240, ASTM A269, ASTM A479, ASTM A262, MSRR 5632, PWA 300, PWA F17 LCS |