Saarstahl AG is one of the most significant manufacturers of long products in the world.
Sede
Völklingen,Saarland, Germany
Sitio web
Tipo
Fabricante y procesador
Certifications
IATF 16949
, IEC 17025
, ISO 17025
, ISO 9001
, ISO 14001
, ISO 50001
, ISO 45001
Grade | Shape | ||
---|---|---|---|
AFNOR 51CDV4 | Rod, Bar | AFNOR 51CDV4, EN 52CrMoV4, EN 51CrMoV4, EN 1.7701 | DIN 17221 |
AFNOR 60SC7 | Rod, Bar | AFNOR 60SC7, SAE 9262, EN 61SiCr7, EN 60SiCr7, EN 1.7108 | DIN 17221 |
BS 251A58 | Rod, Bar | BS 251A58, AFNOR 55Si7RR, AFNOR 56SC7, SAE 9255, EN 56Si7, EN 55Si7, EN 1.5026 | DIN EN 10132 |
BS 523M15 | Bar, Screw, Bolt, Nut, Rivet | BS 523M15, AFNOR 15C2, SAE 5015, EN 15Cr3, EN 1.7015 | |
BS 525A58 | Rod, Bar | BS 525A58, BS 525H60, AFNOR 55C3, SAE 5155, SAE 5160, EN 55Cr3, EN 1.7176 | DIN 17221 |
BS 735A51 | Rod, Bar | BS 735A51, BS 735M50, BS 735H51, AFNOR 50CrV4, AFNOR 51CV4, SAE 6150, EN 51CrV4, EN 1.8159 | DIN EN 10083 |
DIN C35EC | Bar, Screw, Bolt, Nut, Rivet | DIN C35EC, EN Cq35, EN 1.1172 | DIN EN 10263 |
EN 1.7015 | Bar | EN 1.7015, BS 523M15, AFNOR 15C2, SAE 5015, EN 15Cr3 | |
EN 1.8152 | Rod, Bar | EN 1.8152 | |
EN 13NiCr6Pb | Bar | EN 13NiCr6Pb, EN 13NiCr6, EN 16NiCrS4, AFNOR 10NC6, SAE 3115, EN 1.7168 | |