SACAL - Società Aluminum Carisio, today boasts a leadership position in aluminum refining, confirming a traditional presence in the sector, thus obtaining the result of being able to present to the end user the absolute widest range of secondary aluminum alloys for foundries.
Sede
Carisio,Vercelli, Italy
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
EN AB-21000 | Ingot | EN AB-21000, EN AB-AlCu4MgTi | |
EN AB-41000 | Ingot | EN AB-41000, EN AB-AlSi2MgTi | |
EN AB-42000 | Ingot | EN AB-42000, EN AB-AlSi7Mg | |
EN AB-43000 | Ingot | EN AB-43000, EN AB-AlSi10Mg(A) | |
EN AB-43100 | Ingot | EN AB-43100, EN AB-AlSi10Mg(B) | |
EN AB-43200 | Ingot | EN AB-43200, EN AB-AlSi10Mg(Cu) | |
EN AB-43400 | Ingot | EN AB-43400, EN AB-AlSi10Mg(Fe) | |
EN AB-44100 | Ingot | EN AB-44100, EN AB-AlSi12(B) | |
EN AB-44200 | Ingot | EN AB-44200, EN AB-AlSi12(A) | |
EN AB-44300 | Ingot | EN AB-44300, EN AB-AlSi12(Fe) | |