The company's products include over 80,000 off-the-shelf items, including: sheets, cylinders, pipes, screws, pipe fittings, faucets, pumps, rods, profiles, nets, grids and more.All of the above products are marketed by the company in a variety of metals: aluminum, steel, stainless steel (PLBM), nickel alloys, brass, copper, bronze, titanium and lead, as well as engineering plastics products.
Sede
Bnei Ayish, Israel
Sitio web
Tipo
Fabricante y procesador
Certifications
AS 9100
, ISO 9001
Grade | Shape | ||
---|---|---|---|
AISI 301 | Sheet | AISI 301, EN 1.4310 | |
AISI 302 | Sheet, Strip | AISI 302, EN 1.4319 | |
AISI 303 | Plate, Bar | AISI 303, EN 1.4305 | |
AISI 304 | Plate, Sheet, Coil, Strip, Bar, Tube, Profile | AISI 304, EN 1.4301 | |
AISI 304L | Plate, Sheet, Coil, Strip, Bar, Profile | AISI 304L, EN 1.4306 | |
AISI 309 | Plate, Sheet, Coil, Strip | AISI 309, EN 1.4829 | |
AISI 310S | Plate, Sheet, Coil, Bar | AISI 310S, EN 1.4842 | |
AISI 316 | Plate, Sheet, Coil, Strip, Bar, Tube, Profile | AISI 316, EN 1.4436 | |
AISI 316L | Plate, Coil, Strip, Bar, Profile, Sheet | AISI 316L, EN 1.4404 | |
AISI 316Ti | Plate, Sheet, Coil, Strip, Bar | AISI 316Ti, EN 1.4571 | |