Grade | Shape | ||
---|---|---|---|
EN AB-42000 | Ingot | EN AB-42000, EN AB-AlSi7Mg | EN 1676 |
EN AB-43000 | Ingot | EN AB-43000, EN AB-AlSi10Mg(A) | EN 1676 |
EN AB-43100 | Ingot | EN AB-43100, EN AB-AlSi10Mg(B) | EN 1676 |
EN AB-43200 | Ingot | EN AB-43200, EN AB-AlSi10Mg(Cu) | EN 1676 |
EN AB-43400 | Ingot | EN AB-43400, EN AB-AlSi10Mg(Fe) | EN 1676 |
EN AB-44100 | Ingot | EN AB-44100, EN AB-AlSi12(B) | EN 1676 |
EN AB-44200 | Ingot | EN AB-44200, EN AB-AlSi12(A) | EN 1676 |
EN AB-44300 | Ingot | EN AB-44300, EN AB-AlSi12(Fe) | EN 1676 |
EN AB-44400 | Ingot | EN AB-44400, EN AB-AlSi9 | EN 1676 |
EN AB-44500 | Ingot | EN AB-44500, EN AB-AlSi12(Fe) | EN 1676 |