A leading global producer of Precision Seamless Tubes.
Sede
STORFORS, Sweden
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 14001
, ISO 9001
, EN 10305-2
Grade | Shape | ||
---|---|---|---|
Structo 525 | Tube | EN E355, AISI 1524, DIN St 52.0, AFNOR TU52 | EN 10305 |
Structo 620 | Tube | EN E410, DIN StE 460, AFNOR 20MnV6 | EN 10305 |
Structo 720 | Tube | EN E410, DIN StE 460, AFNOR 20MnV6 | EN 10305 |