Grade | Shape | ||
---|---|---|---|
AFNOR 15CDV16 | Bar, Disc | AFNOR 15CDV16, EN 1.7734, EN 15CrMoV6 | |
AISI 8620 | Bar, Disc | AISI 8620, EN 1.6523 | |
AISI 8627H | Bar, Disc | AISI 8627H | |
ASTM F11 | Bar, Disc | ASTM F11, EN 1.7338 | ASTM A182 |
ASTM F5 | Bar, Disc | ASTM F5 | ASTM A182 |
ASTM F9 | Bar, Disc | ASTM F9 | ASTM A182 |
ASTM LF2 | Bar, Disc | ASTM LF2 | ASTM A350 |
BS 709M40 | Bar, Disc | BS 709M40, EN 1.7225 | |
BS 817M40 | Bar, Disc | BS 817M40 | |
DIN 100CrMo7-3 | Bar, Disc | DIN 100CrMo7-3, EN 1.3536 | |