The main product portfolio consists mainly of long rolled products - rolled wire, shaped steel, special bar steel, drawn steel, rails, wide steel, seamless tubes and metallurgical semi-finished products. Other products are coke and accompanying products arising from its production, as well as artificial compacted aggregates and granulated slag.
Sede
Třinec, Czechia
Sitio web
Tipo
Fabricante y procesador
Certifications
ISO 9001
, ISO 14001
, IATF 16949
, ISO 50001
Grade | Shape | ||
---|---|---|---|
DIN 1.7131 | Wire, Bar, Rod | DIN 1.7131, EN 16MnCr5 | |
DIN 1.7147 | Wire, Bar, Rod | DIN 1.7147, EN 20MnCr5, EN 20MnCrB5 | |
DIN QSt 52-3 | Wire, Bar, Rod | DIN QSt 52-3, DIN 1.0569 | |
DIN StE 355 | Wire, Bar, Rod | DIN StE 355, DIN 1.0566 | |
EN 100Cr6 | Wire, Bar, Rod | EN 100Cr6, DIN 1.3505 | |
EN 100CrMnSi6-4 | Wire, Bar, Rod | EN 100CrMnSi6-4, DIN 1.3520 | |
EN 100CrMo7 | Wire, Bar, Rod | EN 100CrMo7, DIN 1.3537 | |
EN 100CrMo7-3 | Wire, Bar, Rod | EN 100CrMo7-3, DIN 1.3536 | |
EN 10CrMo9-10 | Wire, Bar, Rod | EN 10CrMo9-10, DIN 1.7380 | |
EN 11SMn30 | Wire, Bar, Rod | EN 11SMn30, DIN 1.0715 | |